CRYTUR grows Ytterbium doped lutetium aluminium garnet (Yb:LuAG) crystals using the Czochralski growth method. A special protective atmosphere applied during crystal growth and post growth annealing result in a very good lasing efficiency of our crystals. Our production line covers crystal growth, machining and coating technologies.
Technical parameters
Yb:LuAG is very promising Yb-doped laser material. The optical and mechanical properties of LuAG are very similar to YAG crystal. Thanks to similar atomic weight and ionic size of doping Yb3+ ions and substituted Lu3+ lattice ions, the doping concentration has a low influence on lattice vibration modes of LuAG which allow to obtain highly doped Yb:LuAG laser crystal without significant influence on thermal conductivity of this material.
| Material characteristics | |
|---|---|
| Crystal structure | cubic - la3d |
| Emission wavelength | 1031 nm |
| Pump bands | 940 nm, 968 nm |
| Refractive index at 632 nm | 1.84 |
| Absorption cross section at 938 nm | 7.2 x 10-21 cm2 |
| Emission cross section at 1031 nm | 2.6 x 10-20 cm2 |
Generation characteristics
![]() |
![]() |
![]() |
![]() |
Material properties
| Crystal structure | cubic - la3d |
| Emission wavelength | 1031 nm |
| Pump bands | 940 nm, 968 nm |
| Refractive index at 632 nm | 1.84 |
| Absorption cross section at 938 nm | 7.2 x 10-21 cm2 |
| Emission cross section at 2031 nm | 2.6 x 10-20 cm2 |