CRYTUR grows neodymium doped yttrium aluminium garnet (Nd:YAG) crystals using the Czochralski growth method. A special protective atmosphere applied during crystal growth and post growth annealing result in a very good lasing efficiency of our crystals. Our production line covers crystal growth, machining and coating technologies.
Key parameters
Standard production of Nd:YAG laser rods includes:
- Nd dopant concentrations from 0.05 % up to 1.3 at. % of Nd/Y
- Rod diameters from 2 mm up to 12 mm
- Rod lengths of up to 160 mm
- Barrel surface fine ground, polished or grooved
- Perpendicular or wedged ends
- Polishing according to DIN and MIL standards
- A wide variety of anti-reflection, partial or high reflection coatings
- AR coatings with R < 0.2 % and damage threshold higher than 15 J/cm2 for 10 ns pulses
We also offer composite laser rods consisting of doped and undoped segments. These composite rods help to decrease thermal lensing and other thermal stress induced effects, particularly when used in axially diode pumped resonators.

Material properties
| Host | Yttrium aluminium garnet (Y3Al5O12) | ||
| Dopant | Nd3+ | ||
| Crystal structure | cubic | ||
| Unit cell dimensions | ac=1.201 nm | ||
| Refractive index at 1064 nm | 1.816 | ||
| Thermal expansion coefficient | 7.8 x 10-6/K | ||
| Thermal conductivity | 11 W/m K | ||
| Density | 4.56 g/cm3 | ||
| Hardness by Mohs | 8.25 | ||
| Fluorescent lifetime (1% Nd) | 235 µs | ||
| Linear dispersion δn/δT [10-6K-1] | 9.86 | ||
| Pump wavelength | 808 nm | ||
| Laser wavelengths | 4F3/2→4I9/2 | 946 nm | |
| 4F3/2→4I11/2 | 1064 nm | ||
| 4F3/2→4I13/2 | 1319 nm | ||
| 4F3/2→4I13/2 | 1444 nm | ||
| Emission cross section [10-19 cm2] | 1064 nm | 1319 nm | 1444 nm |
| 3.8 | 0.95 | 0.45 | |